Nonwoven web and method of forming same
Abstract
A nonwoven web (32) suitable as a barrier layer in an SMS fabric laminate (12) is provided. The web is formed at commercially acceptable polymer melt throughputs (greater than 3 PIH) by using a reactor granule polyolefin, preferably polypropylene, that has been modified by the addition of peroxide in amounts ranging from up to 3000 ppm to reduce the molecular weight distribution from an initial molecular weight distribution of from 4.0 to 4.5 Mw/Mn to a range of from 2.2 to 3.5 Mw/Mn. Also the addition of peroxide increases the melt flow rate (lowers viscosity) to a range between 800 up to 5000 gms/10 min at 230°C. The resulting web has an average fiber size of from 1 to 3 µm and pore sizes distributed predominantly in the range from 7 to 12 µm, with a lesser amount of pores from 12 to 25 µm, with virtually no pores greater than 25 µm, and with the peak of the pore size distribution less than 10 µm.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 52.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 52 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,849,241 A | Non-woven mats by melt blowing | 1974 | 2,602 |
| EP 0,316,195 A2 | Polyallylene Sulfide nonwoven fabric | — | 15 |
| EP 0,370,835 A2 | Nonwoven continuously-bonded trilaminate | — | 40 |