A method of presulfiding a hydrotreating hydrocracking or tail gas treating catalyst
Abstract
An improved method of presulfiding a hydrotreating or hydrocracking catalyst which minimizes sulfur stripping upon start-up of a hydrotreating or hydrocracking reactor utilizing such a catalyst. The method comprises the steps of contacting a hydrotreating or hydrocracking catalyst with elemental sulfur at a temperature below the melting point of sulfur, thereby forming a sulfur-catalyst mixture, and heating the sulfur-catalyst mixture to a temperature above the melting point of sulfur. Preferably, the sulfur-catalyst mixture is first mixed with at least one member selected from the group consisting of high boiling oils and hydrocarbon solvents to form a prewet mixture prior to heating at a temperature above the melting point of sulfur. Tail gas treating catalysts are also presulfided by these methods.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (4)
Non-Patent Literature (1)
- DERWENT RUSSIAN PATENT REPORT, week C30, section H04, 3rd September 1980, Derwent Publications Ltd, London, GB; & SU-A-701 699 (ELEKTROGORSK. PETROL) 08-12-1979