Shape memory hollow body and method of working the same
Abstract
A shape memory hollow body which is molded from a polyurethane elastomer produced by prepolymer process from a raw material composed of a difunctional diisocyanate, difunctional polyol, and difunctional chain extender containing active hydrogen in a molar ratio of 2.00-1.10 : 1.00 : 1.00-0.10, said polyurethane elastomer containing NCO groups and OH groups in almost equal amounts at the terminals of the polymer chains and having a glass transition point in the range of -50 to 60°C and a crystallinity of 3 to 50 wt%, said hollow body remembering its asmolded basic shape but taking on a deformed shape which is given when it is deformed at a temperature higher than the glass transition point of the polymer and lower than the molding temperature and then set when it is cooled in the deformed state to a temperature lower than the glass transition point. A method of working the above-mentioned shape memory hollow body (1a) remembering its basic shape, said method prising the steps of deforming the hollow body (1a) at a temperature higher than the glass transition point and lower than the molding temperature and then cooling it in the deformed state to a temperature lower than the gl
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 17.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 17 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.