Patents
EP 0,359,209 A2#14616285 Most CitedPendingEuropean Patent Office (EPO)Application

Method and apparatus for using hazardous waste to form non-hazardous aggregate

7Forward Citations (#14616285 Global)
0.2/yrCitation Velocity (#34549315 Global)
2.18Citation PageRank (#12707820 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

Hazardous waste is formed into non-hazardous non-leaching aggregate by introducing the material to a rotary kiln (10) where the large solids are at least partially combusted to form a primary aggregate. Gaseous combustion by-products and waste fines from the waste materials are introduced into at least one oxidizer (26, 56) operating at a temperature in the range of from about 1800° to 2500°F. Under such conditions, some of the waste fines are melted to form a slag-like material that is cooled to form the non-hazardous aggregate. The portion of the material in the ox­idizer that is not melted, is cooled, neutralized and subjected to a solid gas separation. The solid is reintroduced to the ox­idizer with the primary aggregate where they are either melted or entrained within the molten material and become an integral part of the non-hazardous aggregate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 7.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.