Method of making tungsten-titanium sputtering targets
Abstract
Tungsten-titanium sputtering targets with improved characteristics are made from high-purity tungsten powder and a second powder consisting of high-purity titanium hydride powder or high-purity titanium hydride powder and high-purity titanium powder. The second powder contains at least 5%, preferably 25% to 100% by weight of titanium hydride powder. A powder mixture having a binodal particle size distribution with respect to the tungsten and second powders is placed under a containment pressure in a die. The die is heated in a vacuum hot-press chamber to a temperature sufficient to dehydride the titanium hydride, and to remove gases and alkali metals. The die is then heated to a second temperature in the range of 1350 to 1550 o C while maintaining the containment pressure and vacuum. A compaction force in the range of 2000 to 5000 psi is then applied to form a compact. The compaction force and vacuum are subsequently released and the compact is cooled. The compact is easily machined to give a sputtering target having a density of at least 95%, preferably, at least 100% of theoretical density, a total gas content of less than 850 ppm, a carbon content of less than 100 ppm and low pa
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,331,476 A | Sputtering targets with low mobile ion contamination | 1982 | 21 |
Non-Patent Literature (1)
- CANADIAN MINING AND METALLURGICAL, no. 454, February 1950, pages 74-87, Montreal, CA; W.E. KUHN et al.: "A study of some alloys of Titanium"