Process for producing polypropylene and stretched polypropylene film
Abstract
A process for producing polypropylene, which comprises preliminarily polymerizing 3-methylbutene-1 in the presence of a catalyst system formed from [A] a solid titanium catalyst component containing magnesium, titanium, halogen and polycarboxylic acid esters as essential components, [B] an organoaluminum compound, and [C] an organosilicon compound represented by the general formula R n Si(OR′) 4-n wherein R and R′ represent a hydrocarbon group, and 0<n<4, the amount of the 3-methylbutene-1 preliminarily polymerized being 0.1 to 100 g per gram of the solid titanium catalyst, and thereafter, polymerizing propylene or copolymerizing propylene and an alpha-olefin in the presence of the catalyst used in the preliminary polymerization to such an extent that the amount of the monomer or monomers polymerized is from 1,000 to 100,000 times the amount of the 3-methylbutene-1 preliminarily polymerized. Also provided is a stretched polypropylene film having excellent see-through property with little losses of transparency or rigidity obtained by stretching polypropylene containing 1 to 1,000 weight ppm of 3-methylbutene-1 polymer in at least one direction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 27.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 27 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.