Transparent, impact-resistant thermoplastic mouldings, their preparation and their use
Abstract
The moulding composition contains, based on A + B, A: from 5 to 95% by weight of a block copolymer prepared by anionic polymerisation, comprising from 40 to 95% by weight of styrene and from 60 to 5% by weight of butadiene, the block copolymer being selected from the group comprising linear block copolymers, branched block copolymers and mixtures thereof, and B: from 95 to 5% by weight of at least one further, styrene-containing copolymer, and is characterised in that a copolymer B is used which contains from 97 to 55% by weight of styrene and from 3 to 45% by weight of methyl methacrylate copolymerised in a random distribution. The moulding composition is used to produce mouldings.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 11.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (0)