Process for the production of crystalline sodium silicates having a layer structure
Abstract
Crystalline sodium silicates having a layered structure and a molar SiO2:Na2O ratio of 1.9:1 to 3.5:1 are prepared from water glass solutions having a solids content of 20 to 65 % by weight by first treating the water glass solutions in a spray-drying zone. This gives a pulverulent amorphous sodium silicate having a maximum loss on ignition of 20 % by weight, while the waste gas leaving the spray drying zone has a temperature of at least 140 DEG C. The spray-dried sodium silicate is then heat treated in an ignition zone having a movable solid bed at temperatures of 500 to 800 DEG C for 1 to 60 minutes in the presence of at least 10 percent by weight of recycled material. This recycled material was obtained by mechanical comminution of crystalline sodium silicate discharged from the ignition zone.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.