High rate tungsten CVD process for stress-free films
Abstract
A method is described for depositing thick, low-stress refractory metal films on a substrate. For example, a layer of tungsten of any required thickness may be deposited by the silicon reduction of tungsten hexafluoride in a CVD reactor. This is accomplished by alternating the process step of plasma depositing an amorphous silicon film, with the process step of exposing the silicon film to tungsten hexafluoride until the required thickness of tungsten is reached. The thickness of the deposited amorphous silicon film must be less than the thickness at which the conversion of silicon to tungsten becomes self-limiting to assure that all of the amorphous silicon is converted. The bombardment of the silicon during the plasma deposition "hammers" the underlying tungsten film and relieves the stress in the film.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (4)
| Patent | Title | Year | Citations |
|---|