Heat resisting low expansion zirconyl phosphate-zircon composite bodies and process for producing the same
Abstract
Heat resisting low expansion zirconyl phosphate-zircon composite bodies are disclosed, which contain zirconyl phosphate and zircon as a main crystalline phase and a secondary crystalline phase, respectively. The heat resisting low expansion zirconyl phosphate-zircon composite bodies have a coefficient of thermal expansion in a temperature range from room temperature to 1,400°C being not more than 30×10⁻⁷/°C and a melting point being not less than 1,600°C. The composite bodies have a chemical composition essentially consisting of 58.2 to 65.4% by weight of ZrO₂, 17.4 to 37.1% by weight of P₂O₅, and 1.5 to 19.0% by weight of SiO₂. The heat resisting low expansion zirconyl phosphate-zircon composite bodies optionally contain MgO and Aℓ₂O₃ in a total amount of not more than 2.5% by weight or 0.1 to 4% by weight of Nb₂O₅. A process for producing such zirconyl phosphate-zircon composite bodies is also disclosed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.