Breathable film and process for production of the same
Abstract
A linear polyethylene (100 wt parts) of low density of 0.870 to 0.915 g/cc and containing 15 to 50 wt% of components extractable with xylene at 25±1°C and a weight average molecular chain length of 1,000 - 9,000 Ångstroms is mixed with 50-400 parts of an organic or inorganic filler (e.g. calcium carbonate, barium sulfate or talc) and optionally to help dispersion of the filler 0.5-8 parts of a nonionic surfactant (e.g. a glycerine or sorbitan ester of a C12-22 fatty acid) and the mixture is molded into a film. The film is stretched either (a) uniaxially at 30-80°C at a stretch ratio of 1.2-8 in the mechanical direction or (b) biaxially at 40-100°C at a ratio of 1.1-8.0 in the mechanical direction and then at 70-100°C at a ratio of not above 6.0 transversely; optionally a heating setting treatment is then applied. The resultant film formed from the stretched composition is breathable to a high extent and has good strength, touch and appearance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 23.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 23 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.