Silicon nitride sintered bodies and process for manufacturing the same

10Forward Citations (#9960198 Global)
0.3/yrCitation Velocity (#27905968 Global)
3.01Citation PageRank (#7546962 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

Silicon nitride sintered bodies of high strength at high temperature comprise not less than 70% by weight of Si₃N₄ and essentially consist of Si, O, N and a remainder being at least two of the rare earth elements Y, Er, Tm, Yb and Lu. The ratio of the molar amount of all the rare earth elements when calculated as Ln₂O₃ in which Ln is Y, Er, Tm, Yb or Lu to the molar amount of oxygen when calculated as SiO₂ is in a range from 0.4 to 1.3. The amount of oxygen when calculated as SiO₂ is obtained by subtracting the amount of oxygen in all the Ln₂O₃ from the amount of oxygen in the sintered body and expressing the remaining amount of oxygen as SiO₂ . Each of the rare earth elements is not more than 95 mol% of the sum of all the rare earth elements in the sintered body. The intergranular phase of the Si₃N₄ grains is substantially a crystalline phase of which not less than 50% is a crystalline phase of an apatite structure. Such bodies can be made by pressureless sintering or sintering in a pressurized atmosphere.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 10.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.