EP 0,243,614 A3#152888802 Most CitedExpiredEuropean Patent Office (EPO)Utility

Refractory composition and refractory brick made thereof

0Forward Citations (#152888802 Global)
0.0/yrCitation Velocity (#152888802 Global)
0.56Citation PageRank (#152888802 Global)
2Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The composition, especially for a refractory brick for lining rotary kilns in the cement industry, is based on magnesia spinel, having a content of 10 to 50 % by weight of spinel clinker (MgO.Al2O3), 50 to 90 % by weight of sintered magnesia and a content of 0.5 to 4 % by weight, relative to the total quantity of spinel clinker and sintered magnesia, taken as 100 % by weight, of a metal oxide which promotes attachment, the metal oxide being zirconium oxide in a grain size range of < 0.1 mm; a refractory brick is produced using such a refractory composition. <IMAGE>

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (2)