Process for preparing porous film or sheet
Abstract
process for preparing a porous film or sheet, which process comprises melt-forming a composition into a film or sheet and then stretching the thus-formed film or sheet at a temperature in the range of 30° to 110°C, said composition containing: (a) 30-90% by weight of a linear low-density polyethylene having a density not smaller than 0.910 g/cm 3 and smaller than 0.940 g/cm 3 ; (b) 10-70% by weight of an ethyleneia-olefin copolymer having a density not smaller than 0.860 g/cm 3 and smaller than 0.910 g/cm 3 , a boiling n-hexane insolubles content not less than 10% by weight and a maximum peak temperature not lower than 100°C as measured according to a differential scanning calorimetry; and (c) 20-500 parts by weight of a filler based on 100 parts by weight of said resin components.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 12.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.