Electrodeposition of an iron-zinc alloy coating
Abstract
In the electrodeposition of iron-zinc alloy coatings, a lustrous, adherent iron-zinc coating containing 10-20% iron is achieved over a current density range of 43-172 amps/dm2 and line speeds of 30.4-152 m/min. employing an electrolyte maintained at a temperature of 54.4 to 71.1oC which contains FeCl2, ZnCl2, KCl, K2SO4, a chelating agent such as citric acid, and a minor amount of an adduct composed primarily of polyalkylene glycols.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (2)
- Content of paper by T.Irie et al presented at 4th AES , Chicago , 1984 ( file pp 39-62 )
- pp 72-73 of the file ( electrolyte constitution for experiments illustrated in Figs 1 , 2 ).