EP 0,202,793 A2#10344058 Most CitedPendingEuropean Patent Office (EPO)Application

Method of weld repairing steam turbine rotors

10Forward Citations (#10344058 Global)
0.2/yrCitation Velocity (#28214825 Global)
2.21Citation PageRank (#12376413 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

Method for effecting weld repairs to a nickel-molybdenum-vanadium steel steam turbine rotor. One or more weld passes are made using a filler metal to repair a defect in the rotor. A filler metal alloy is prepared consisting essentially of, by weight, per cent 0.090-1.110 carbon, 1.25-1.80 manganese, up to 0.0010 phosphorus, up to 0.010 sulfur, 0.20-0.50 silicon, 1.40-2.10 nickel, up to 0.30 chromium, 0.25-0.55 molybdenum, up to 0.05 vanadium, up to 0.10 titanium, up to 0.10 zirconium, up to 0.10 aluminum, up to 0.20 copper, up to 0.0015 antimony, up to 0.015 tin, up to 0.020 arsenic, and, up to, in ppm, 35 oxygen, 25 nitrogen, and 10 hydrogen, the balance being iron. This alloy is vacuum induction melted. Preferably this alloy has 0.10-0.25 chromium and a maximum of 0.010 zirconium. Welds using this filler metal exceed the rotor base material in strength, notch toughness, and resistance to temper embrittlement.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 10.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.