Patents
EP 0,187,007 A2#5149130 Most CitedPendingEuropean Patent Office (EPO)Application

Porous mullite

17Forward Citations (#5149130 Global)
0.4/yrCitation Velocity (#18581426 Global)
4.79Citation PageRank (#3550680 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

Clay, preferalby kaolin, is calcined through its exotherm, but without substantial mullite formation [e.g., 1 hour at 1000°C]. The calcined clay is leached with an alkaline aqueous solution to remove [i.e., leach] silica. If the molar A1 2 0 3 /Si0 2 ratio is < 3/2 the final product will contain mullite plus excess SiO 2 and if the A1 2 0 3 /Si0 2 ratio is < 3/2, the final product will contain excess Al 2 O 3 . The leached clay is washed, preferably under acid conditions at about pH 3-5, to remove excess alkali ions; and then dried. The washed clay is then calcined at conditions to produce mullite [e.g., 3 hours at 1250°F]. Materials made in this manner exhibit high pore volume despite the final high temperature heat treatment and suitable for catalyst and sorbent applications.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 17.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.