Method of producing austempered spheroidal graphite cast iron body
Abstract
57 An excellently austempered spheroidal graphite cast iron body, which may be a thick-wall body, is obtained by using a spheroidal graphite cast iron composition consisting essentially of 3.0-4.0 wt% of C, 1.5-3.0 wt% of Si, 0.3-0.8 wt% of Mn, 0.3-2.0 wt% of Cu, 0.005-0.2 wt% of a spheroidizing agent such as Mg, Ca or Ce, 0-0.1 wt% of Mo, 0-0.3 wt% of Ni and the balance of Fe, and by accomplishing the cooling of the cast iron body from the austenite stabilizing temperature to the bainite transformation temperature at an adequate cooling rate so as to avoid precipitation of pearlite, preferably at a cooling rate between 10°C/sec and 0.64°C/sec. Best results are obtained by performing the cooling in a fluidized bed furnace.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 19.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 19 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.