Patents
EP 0,140,693 A2#8809763 Most CitedPendingEuropean Patent Office (EPO)Application

Electrodes made with disordered active material and methods of making the same

11Forward Citations (#8809763 Global)
0.3/yrCitation Velocity (#27262220 Global)
4.50Citation PageRank (#3932281 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The present invention provides an electrode (15, 115, 165, 225) which uses a disordered active material (15, 115, 165, 225) preferably formed by rapid solidification. The active material does not need a binder to be used as an electrode, and thus, is considered self-supporting. The material also is substantially nonporous or impermeable to an electrolyte and when used as an electrode exhibits an increase in cell capacity with improved resistance to corrosion. An electrochemical cell (10, 85, 100, 150, 200) and battery (75) utilizing an electrode of the present invention provides greatly improved cycle life and energy density without a significant decrease in cell capacity. Methods of making the electrode by rapidly solidifying a disordered material are also included. A method of assembling an electrochemical cell using a self-supporting electrode includes the step of producing a disordered active material and aligning the material in a predetermined position in a cell casing.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 11.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.

Non-Patent Literature (2)

  • LIEBERMANN ET AL.: "Transactions on Magnetics", vol. 12, 6 November 1976, IEEE, article "Production of Amorphous Alloy Ribbons and Effects of Apparatus Parameters on Ribbon Dimensions"
  • LIEBERMANN: "The Dependence of the Geometry of Glassy Alloy Ribbons on the Chill Block Melt-Spinning Process Parameters", MATERIALS SCIENCE AND ENGINEERING, vol. 43, 1980, pages 203 - 210, XP024085093, DOI: doi:10.1016/0025-5416(80)90103-2