High-silica mordenite and process for preparation thereof

14Forward Citations (#6861741 Global)
0.3/yrCitation Velocity (#22613861 Global)
2.74Citation PageRank (#8772562 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

A high-silica mordenite is provided, which is a synthetic mordenite prepared without performing the dealuminization treatment, and is characterized in that the silica/alumina molar ratio is in the range of from 12 to 30 and the amount of benzene adsorption is 7 to 10% by weight as determined at a temperature of 25 DEG C under a vapor pressure of 35 mmHg. The high-silica mordenite is prepared by a process wherein a reaction mixture having a composition represented by the following oxide molar ratios: Na2/SiO2 = 0.08 - 0.2 SiO2/Al2O = 14 - 55 H2O/Na2O = 100 - 300 and H2O/SiO2 = 10 - 40 is formed using synthetic amorphous silicic acid having an apparent specific gravity of from 0.05 to 0.45 g/ml as a silica source, and the reaction mixture is heated at a temperature of 140 to 180 DEG C with stirring to effect crystallization.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 14.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (14 of 14 total)

References Cited — Backward Prior Art (0)

No backward patent references recorded.