Methods of brazing adjoining surfaces of elements, brazing alloys, and structures comprising brazed joints
Abstract
Brazing of the pins and mounting flanges to electronic chip carrying substrates requires brazing materials which remain solid at the temperatures used to remove and replace chips. The flanges and pins are brazed with an initially eutectic Au:Sn brazing alloys which is modified during brazing by addition of copper to promote formation of the higher melting point phase of the alloy. A Group VIII metal is also added during brazing to draw Sn out of the melt by gettering, further to promote formation of the phase of the alloy and to thicken the braze material. As shown a multilayer substrate 10 has a molybdenum pad 11 coated with a protective layer of nickel 12. A relatively thick copper layer 13 (0.0002 - 0.0025 cms) is coated with a very thin (up to 1.25 µm) layer of nickel 14 to serve as tin gettering metal A braze fillet 15 of Au80:Sn20 is positioned on the layer 14 and surrounds the nickel plating 17 on Kovar pin 19. When the joint is brazed at a nominal temperature of 395°C the copper 13 and nickel 14 react with the braze fillet material and on cooling, the brazed joint material has a raized melting point.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.