Process for making a tempered glas dielectric material for an electical isolator, and isolator obtained
Abstract
A tempered glass dielectric material for use as an electrical insulator is thermally tempered to produce surface compression between 200 MPa and 400 MPa. At least part of the material is then chemically tempered under conditions of temperature and duration such that the surface compression due to the thermal tempering is reduced by between 50% and 80%. The chemical tempering is effected by applying to the relevant part of the material, at ambient temperature, a solution containing alkaline salts. This solution is dried and the material then heated for several hours at a temperature between 300 DEG C. and 500 DEG C. The solution has the following composition (in percentage by weight): -H2O 70% to 90% -Starch 2% to 10% -KNO3 4% to 12% - K2HPO4 + KCl + K2SO4 4% to 20% -
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.