Process for preparing latices having a high nitrile rubber content
Abstract
1. Process for the production of nitrile rubber latices, the solids thereof having a Defo value of between 5 and 50 N, from 40 to 60% by weight of butadiene and/or isoprene, 40 to 60% by weight of acrylonitrile and/or methacrylonitrile, 0 to 15% by weight of styrene and 0 to 10% by weight of alpha,beta-monoethylenically unsaturated carboxylic acids by polymerisation in a ratio of water to monomers of 3 : 1 to 1 : 1 in a primary method of operation up to a conversion of the monomers of at least 95%, characterised in that polymerisation is carried out at 30 to 50 degrees C in the presence of 0.5 to 1.0% by weight of a long-chain alkyl mercaptan with 8 to 12 carbon atoms, at least 2% by weight of at least one anionogenic surfactant and from 0.2 to 0.8% by weight of an alkali metal and/or ammonium peroxodisulphate, the percentages relating to the total quantity of the monomers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.