Method of chromium-passivated aluminium contact etching with high-duty semi-conductor structures

0Forward Citations (#91219730 Global)
0.0/yrCitation Velocity (#91219730 Global)
0.56Citation PageRank (#91219730 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The goal of the solution is to etch the aluminium contact by passive chrome on power semiconductor structures. The contact layer is selectively etched at the temperature from 30 to 100 degrees Celsius though the photolithographic mask in the etching agent containing from 20 to 30 percent by weight of ferricyanide of potassium and from 10 to 20 percent by weight of potassium hydroxide, which are dissolved in deionised water.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (0)

No backward patent references recorded.