Method of high-duty semi-conductor structures' multi-layer contact etching
Abstract
The goal of the solution is to etch the multiple-layer contact of the power semiconductor structures composed of titanium - silver or titanium - nickel - silver. At first, the contact layers that contain mixed orthophosphoric and nitric acids in the ratio from 25:1 to 5:1 at the temperature from 20 to 100 degrees Celsius are etched, whereupon the contact layers that contain nickel in nitric acid, containing from 1 to 5 percent by weight of hydrochloric acid, at the temperature from 20 to 40 degrees Celsius, are etched. At last, the contact layers containing titanium in hydrochloric acid at the temperature from 20 to 40 degrees Celsius are etched.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.