Patents
CS 273,742 B1#95999291 Most CitedExpiredInternational OfficeUtility

Method of phenolformaldehyde binder preparation for mineral and glass fibrous materials

0Forward Citations (#95999291 Global)
0.0/yrCitation Velocity (#95999291 Global)
0.56Citation PageRank (#95999291 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The binder is produced by multilevel condensation of phenol with formaldehyde in a molar ratio of 1 : 2.3 to 3.5 in the presence of calcium oxide of hydroxide at a temperature up to 85 degrees C. After condensation neutralisation is performed with a solution of mineral acid and carbonic acid. Neutralisation is performed at 0 to 19 degrees C and at the same temperature separation of the indissoluble share occurring during neutralisation is performed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (0)

No backward patent references recorded.