Method of products' eloxal coated surface activation from hardened aluminium alloys and means for realization of this method

0Forward Citations (#105372978 Global)
0.0/yrCitation Velocity (#105372978 Global)
0.56Citation PageRank (#105372978 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The solution applies to the hardening of aluminium alloy surface finishing, mainly for the aircraft industry. The scope of the solution is to increase the adherence of epoxy-based coating compounds to the anodised surface of products made of these alloys for severe operating and climatic conditions. Before the application of the epoxy-based coating itself, the relevant surface is painted by a liquid alkaline agent and then this agent is left to treat the surface and to evaporate in a temperature of 16 - 30 degrees C for 5 - 25 minutes. The agent for this method of surface treatment consists of the following mixture: absolute ethyl alcohol (20 - 30%); ammonium hydroxide water solution (2 - 4%); acetone (70 - 75%).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (0)

No backward patent references recorded.