Abstract

The rubber composition per 100 weight parts of chloroprene rubber in the composition with ethylene-propylene terpolymer contains 1.5 to 15 weight parts of polyvinyl chloride or its copolymer with vinyl acetate, where the volume of vinyl acetate in copolymer is 6 to 30 weight percent, 120 to 250 weight parts of soot or inorganic fillings, 6 to 40 weight parts of mineral oil or esters of dicarboxylic acids, 2 to 20 weight parts of oxidized asphalt, 2 to 20 weight parts of factice, 0.5 to 2 weight parts of stearic acid, 3 to 10 weight parts of zinc oxide, 1 to 7 weight parts of magnesium oxide, 0.1 to 1.5 weight parts of 2-mercaptoimidazoline, 0.3 to 2 weight parts of tetramethylthiuram disulphide, 0.3 to 1.5 weight parts of sulphur, 0.3 to 2 weight parts of 2- mercaptobenzothiazole or 2.2-dibenzothiazyl disulphide, 0.5 to 5 weight parts of paraffin, 0.3 to 1.5 weight parts of phenyl-β- naphthylamine and 0.3 to 1.5 weight parts of N- isopropyl-N-phenyl-p-phenyldiamine. The rubber composition can per 100 weight parts contain 0.1 to 1.5 weight parts of a derivate of diethyldithiocarbamic acid. The rubber damp proof foils, made out of the introduced rubber composition, reach higher param

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (0)

No backward patent references recorded.