Method of grey cast iron production with strength above 300 mpa
Abstract
This concerns the production of a grey perlitic cast iron from predominantly secondary raw material for sophisticated castings with required strength of 300 up to 450 MPa. The cast iron is melted in an electric furnace from a charge containing between 40 and 90 mass % of modular cast iron scrap and between 10 and 40 mass % of plain carbon steel scrap, while the aggregate content of a charge material comes to at least 60 mass %. The remaining portion of the charge material up to 100 mass % is amended with pig iron or grey cast iron scrap or both simultaneously to the resulting phosphorus content in the cast iron of less than 0.07 mass % and sulphur content in the cast iron of less than 0.06 mass %.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.