Patents
CS 196,439 B2#151981626 Most CitedExpiredInternational OfficeUtility

Semi-ferritic stainless steel and heat treatment method

0Forward Citations (#151981626 Global)
0.0/yrCitation Velocity (#151981626 Global)
0.56Citation PageRank (#151981626 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

1306415 Stainless steel UGINE KUHLMANN 29 May 1970 [3 June 1969] 26142/70 Heading C7A Semi-ferritic stainless steel, contains 10-50% austenite in the hot state, comprises:- the balance, apart from impurities (e.g. P), being Fe, and has a Cr equiv [defined as %Cr + %Si + %Mo + 4(%Ti + %Nb] and a Ni equiv [defined as %Ni + %Mn/z + %Cu/z + %Co + 20(%C + %N)] which fall within the area ABCDEA of the Fig. The alloy may be heated at 700‹-900‹C, then (a) slowly cooled (e.g. at a rate of 25‹ C/hr down to 650‹C and then air cooled), or (b) sub-zero treatment (e.g. at -80‹C) or (c) cold worked at ambient temperatures (e.g. with a reduction of 30%), and then annealed at below 850‹C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (0)

No backward patent references recorded.