New process for smelting medium and low carbon ferro-mangenese by blast furnace-refining furnace method

6Forward Citations (#17765638 Global)
0.3/yrCitation Velocity (#27421886 Global)
1.61Citation PageRank (#20454156 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The blast furnace-refining furnace process of smelting medium and low carbon ferromanganese features the molten pool temperature of 1650-1750 deg.c in the refining furnace; raising the temperature of molten ferromanganese from the blast furnace to 1450-1550 deg.c in the hot metal mixer; and blowing oxygen to decarbonize in the refining furnace at front stage oxygen supplying strength of 2.5-3.0 cu m/min, middle stage Ar-O2 mixing blowing of oxygen supplying strength of 0.8-1.0 cu m/min, and later stage Ar blowing reduction and final temperature controlled in 1750-1800 deg.c. The present invention makes it possible to utilize poor manganese ore resource in producing ferromanganese and has low power consumption, high production efficiency and high Mg recovering rate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 6.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.