Patents
CN 104,591,663 A#3845623 Most CitedActiveChina (CNIPA)Utility

Method for fast preparing mine tailing underground filling material

21Forward Citations (#3845623 Global)
1.9/yrCitation Velocity (#2274135 Global)
5.18Citation PageRank (#3126004 Global)
4Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The invention discloses a method for fast preparing a mine tailing underground filling material. The method comprises the following steps of putting mine tailing, a filling base (comprising furnace slag micro-powder, steel slag micro-powder, red mud, fly ash, silica fume, waste gypsum, quicklime and solid sodium silicate) and water into a cement mortar mixer, carrying out mixing, pouring the uniform mixture into a plastic mold, putting the plastic mold into a microwave device with microwave frequency of 915-5800 MHZ, carrying out radiation at microwave output power of 80-800W for 5-30min, putting a test block into a maintenance case, and carrying out maintenance until desired age so that the mine tailing underground filling material satisfying filling requirements is obtained. The mine tailing underground filling material has a low cost, a fast curing rate and strength satisfying requirements on filling and mining under mine, solves the technical problem that the existing mining cementation filling material has a slow curing rate and a high filling cost, is suitable for filling various metal mines suitable for cemented filling mining and provides a novel feasible approach for resou

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 21.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 21 total)

PatentTitleYearCitations
CN 107,975,044 AA kind of method that Caving Method with Large Space mine is backfilled using tailing surface subsidence hole—7
CN 111,138,099 ACuring agent for phosphogypsum waste residues and curing method thereof—8
CN 114,183,192 AFilling method of underground goaf of nonferrous metal mine, treatment method of tailing slurry of nonferrous metal mine and biomass-based cementing material—1
CN 111,118,238 AMethod for preparing steelmaking furnace burden by using blast furnace gas ash zinc extraction kiln slag—4
CN 109,580,302 AA kind of uniaxial compression experiment tailings paste sample preparation device and experimental method—4
CN 105,753,418 AMine filling cementing material prepared by utilizing industrial by-product gypsum and preparation method for mine filling cementing material—10
CN 112,851,286 AMethod for preparing underground cementing filling material by fully utilizing fine-grained gold tailings—1
CN 108,101,484 A/ structures reinforcement material is built in a kind of underground—1
CN 114,183,192 BFilling method of nonferrous metal mine underground goaf, processing method of nonferrous metal mine tailing pulp and biomass-based cementing material20240
CN 106,915,941 BHalf water ardealite mine filling material and preparation method thereof20190
CN 113,233,824 APreparation method of tin tailing based low-permeability heavy metal solidified body for underground filling—2
CN 106,495,636 AA kind of tailing foam mortar of underground mine exploitation filling—1
CN 112,321,203 AFormula and process for backfilling mine from bulk solid waste—2
CN 107,975,044 BMethod for backfilling collapse method mine by utilizing tailing surface collapse pits20210
CN 106,915,941 AHalf water ardealite mine filling material and preparation method thereof—5