Method for producing alumina clinker
Abstract
The invention discloses a method for producing alumina clinker. According to the method, alumina clinker is prepared by calcining in a rotary kiln, and control over the phase of alumina clinker is realized by controlling the mixture ratio of limestone to high-alumina fly ash, pre-decomposing and preheating outside the kiln, calcining in the rotary kiln and controlling conditions such as the pre-decomposing rate as well as ventilation, calcining temperature and calcining atmosphere in a calcining process. The temperature of a reaction region is only 1,100-1,500 DEG C, and phases of final alumina clinker mainly include CaO.Al2O3, 2CaO.SiO2 and sillico aluminate minerals such as 12CaO.7Al2O3 and the like. Alumina clinker undergoes autogenous pulverization due to crystal transfer in a cooling process, and finished alumina clinker is prepared from autogenously-pulverized alumina clinker with an alkaline leaching method.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗