High-strength, cold-formable steel and flat steel product made from such steel
Abstract
High-strength, cold-formable steel and a flat steel product produced from such a steel, in which an optimal combination of weldability and a low tendency towards delayed cracking is ensured along with good strength and hot and cold deformability. In order to achieve this, a steel according to the invention contains (in % by weight) C: 0.1 - 1.0%, Mn: 10 - 25%, Si: up to 0.5%, Al: 0.3 - 2%, Cr: 1.5 - 3.5%, S: < 0.03%, P: < 0.08%, N: < 0.1%, Mo: < 2%, B: < 0.01%, Ni: < 8%, Cu: < 5%, Ca: up to 0.015%, at least one element from the group "V, Nb" with the following proviso: Nb: 0.01 -0.5%, V: 0.01 - 0.5% and optionally Ti: 0.01 - 0.5% and iron and unavoidable, production-related impurities as the remainder.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.