Homogenization of martensitic stainless steel after remelting under a layer of slag
Abstract
The present invention relates to a method for producing a martensitic stainless steel that includes a step in which an ingot of the steel is remelted under a layer of slag, followed by a step in which the ingot is cooled. Before the skin temperature of the ingot resulting from the slag remelting step drops below the martensitic transformation temperature Ms of the steel, the ingot is placed in a furnace, the initial temperature T0 of which is then above the cooling-induced pearlite transformation finish temperature Ar1 of the steel. In the furnace, the ingot is subjected to a homogenization treatment at least for a holding time t after the temperature of the coolest point in the ingot has reached a homogenization temperature T, said holding time t being equal to at least one hour and the homogenization temperature T varying between approximately 900°C and the burning temperature of the steel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.