Method for manufacturing a casting-die body and a casting-die body
Abstract
A casting-die body (1) made of a hardenable copper alloy is provided with an inner wear-protective layer (7) of chromium whose hardness decreases from the billet-side surface (8) in the direction of the casting-die body (1). The wear-protective layer (7) is made up of two chromium layers (9, 10). For this purpose, the casting-die body (1) is given a solution heat treatment, is chromium plated, and is then hardened, as a result of which the initially very high hardness of the chromium layer (9) is reduced. The hardness of the chromium layer (9) then is about 650 HV. Subsequently, to increase the wear protection, the second chromium layer (10) is applied. The result is a conventional chromium-plated layer having a hardness of between 850 HV and 1050 HV.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.