Asphaltic foam
Abstract
An asphaltic polyurethane or isocyanurate foam (12) useful in roofing applications. The foam is made from asphalt having a penetration range of between approximately 5-25, a softening point of between approximately 120 .degree.F and 200 .degree.F, and an asphaltene content of no more than about 30 %. This asphalt is liquified and mixed with a mixture of polyols such as Voranol 270, Multranol 9138, and castor oil. Other chemicals, such as a surfactant, a viscosity reducer, and a flame retardant can also be included in this mixture. The mixture is then brought to a temperature of between approximately 140 .degree.F and 220 .degree.F, mixed with water and a polyisocyanate in a molar ratio of polyisocyanate:polyol of between about 0.95:1 and about 1.3:1, and reacted t o form an asphaltic polyurethane foam. Alternatively, a molar ratio of polyisocyanate:polyol of between about 2.0:1 and about 2.7:1 can be used. In this case, an asphaltic isocyanurate foam is produced.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.