Process for producing stereoregular polymers having a narrow molecular weight distribution
Abstract
ABSTRACT OF THE DISCLOSURE Stereoregular polymers having a molecular weight distribution of less than 5.0 and an isotactic index in excess of 96 percent are produced by polymerizing an alpha-olefin having 3 to B carbon atoms in a low pressure gas phase fluid bed process at a temperature in excess of 80°C employing a heat stable catalyst system comprising (a) a solid catalyst component containing magnesium, titanium, halide and a polycarboxylic acid ester containing two coplanar ester groups attached to adjacent carbon atoms, as inside electron donor, (b) an organoaluminum cocatalyst, and (c) a silicon compound containing a silicon-oxygen-carbon linkage, as out-side electron donor.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.