Process for producing a sealing layer
Abstract
The invention describes a process for producing a horizontal, vertical or inclined sealing layer, in which at least one hydraulically curing binder, if desired in admixture with swellable clay minerals and/or inert aggregates, in particular ground rock, and/or coarse aggregates larger than 1 mm, preferably sands and gravels, and also, if desired, with further additives which increase the impermeability of the sealing layer towards environmentally relevant liquids, is introduced as sealing material to form the sealing layer together with an amount of water which is less than 60%, preferably less than 30%, of the water required for complete hydration of the hydraulic binder or, if swellable clay minerals are present, the water required for hydration of the hydraulic binder and additionally for swelling these clay minerals, and the sealing material is allowed to cure or swell over the course of time by reaction with moisture only after introduction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗