Patents
US 5,984,159 A#248246 Most Cited · 98 citations3.6/yr · PR 11.40ExpiredUS · Utility
Method and apparatus for cutting through a flat workpiece made of brittle material, especially glass
Inventors: Ostendarp Heinrich, Hermanns Christoph, Hauer Dirk, Stein Juergen, Geissler GeorgAssignee: Schott GlasFiled 1998-04-14 · Granted 1999-11-16

The method and apparatus for cutting through flat workpieces made of glass can cut through workpieces with greater thickness, e.g. glass panes with a thickness greater than 0.2 mm, than possible up to now with a comparable known method, without micro-fractures, glass fragments…

US 6,112,967 A#626703 Most Cited · 62 citations2.4/yr · PR 6.71ExpiredUS · Utility
Method and apparatus for cutting through a flat workpiece made of brittle material, especially glass
Inventors: Ostendarp Heinrich, Hermanns Christoph, Hauer Dirk, Stein Juergen, Geissler GeorgAssignee: Schott GlasFiled 1999-06-23 · Granted 2000-09-05

The method and apparatus for cutting through flat workpieces made of glass can cut through workpieces with greater thickness, e.g. glass panes with a thickness greater than 0.2 mm, than possible up to now with a comparable known method, without micro-fractures, glass fragments…

EP 0,872,303 A2#1129564 Most Cited · 45 citations1.6/yr · PR 7.29PendingEP · Application
Process and apparatus for splitting flat pieces of brittle material, particularly of glass

The method involves a relative motion of the workpiece material (1) and a symmetric heat radiation spot (3) along a separation line (2), with subsequent cooling of the heated separation line section. The heat radiation spot has a higher radiation intensity on its edge zone and a…

JP H1121141 A#5114146 Most Cited · 17 citations0.6/yr · PR 6.16ExpiredJP · Utility
Method for cutting brittle material, more particularly flat processed articles made of glass and device therefor

PROBLEM TO BE SOLVED: To provide a method for cutting a flat processed article, for example, a glass sheet thicker than 0.2 mm, without the occurrence of microcracks and the breaking or fissuring of glass and a device therefor. SOLUTION: This method consists in a) heating the…

EP 0,872,303 B1#7784703 Most Cited · 13 citations0.6/yr · PR 1.97ExpiredEP · Utility
Process and apparatus for splitting flat pieces of brittle material, particularly of glass

The method involves a relative motion of the workpiece material (1) and a symmetric heat radiation spot (3) along a separation line (2), with subsequent cooling of the heated separation line section. The heat radiation spot has a higher radiation intensity on its edge zone and a…

DE 59,808,669 D1#71649934 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Verfahren und Vorrichtung zum Durchtrennen von flachen Werkstücken aus sprödem Material, insbesondere aus Glas
Inventors: Ostendarp Dr, Stein Juergen, Hermanns Dr, Hauer Dirk, Geissler Heinz-georgAssignee: Schott GlasFiled 1998-04-09 · Granted 2003-07-17

The method involves a relative motion of the workpiece material (1) and a symmetric heat radiation spot (3) along a separation line (2), with subsequent cooling of the heated separation line section. The heat radiation spot has a higher radiation intensity on its edge zone and a…

HK 1,017,335 A1#105881559 Most Cited · 0 citations0.0/yr · PR 0.56PendingHK · Application
Method and apparatus for cutting through a flat workpiece made of brittle material, especially glass

The method involves a relative motion of the workpiece material (1) and a symmetric heat radiation spot (3) along a separation line (2), with subsequent cooling of the heated separation line section. The heat radiation spot has a higher radiation intensity on its edge zone and a…

MY 120,533 A#101114444 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredMY · Utility
Method and apparatus for cutting through a flat workpiece made of brittle material, especially glass.

THE METHOD AND APPARATUS FOR CUTTING THROUGH FLAT WORKPIECES (1) MADE OF GLASS CAN CUT THROUGH WORKPIECES WITH GREATER THICKNESS, E.G. GLASS PANES WITH A THICKNESS GREATER THAN 0.2 MM, THAN POSSIBLE UP TO NOW WITH A COMPARABLE KNOWN METHOD, WITHOUT MICRO-FRACTURES, GLASS…