Microstructured optical fiber and method of making. Glass soot is deposited and then consolidated under conditions which are effective to trap a portion of the consolidation gases in the glass to thereby produce a non-periodic array of voids which may then be used to form a void…
murtagh-michael
Disclosed is an optical fiber having a core with an alkali metal oxide dopant in an peak amount greater than about 0.002 wt. % and less than about 0.1 wt. %. The alkali metal oxide concentration varies with a radius of the optical fiber. By appropriately selecting the…
Microstructured optical fiber and method of making. Glass soot is deposited and then consolidated under conditions which are effective to trap a portion of the consolidation gases in the glass to thereby produce a non-periodic array of voids which may then be used to form a void…
An optical fiber is disclosed in which the core region of the optical fiber is doped with Cl and F in order to reduce the viscosity mismatch between the core region and the adjacent cladding region. In one embodiment of the invention, the optical fiber is a single-mode step…
An optical fiber comprising: a silica based core having a first index of refraction n 1 ; and at least one silica based cladding surrounding the core, the at least one silica based cladding comprising index lowering non-periodic voids containing a gas, wherein at least 80% of…
An optical fiber comprising: a silica based core having a first index of refraction n 1 ; and at least one silica based cladding surrounding the core, the at least one silica based cladding comprising index lowering non-periodic voids containing a gas, wherein at least 80% of…
The present invention relates to a process for manufacturing flat sheets of a glass-based material and to an apparatus therefor. The process comprises providing a glass preform, heating the glass preform in a furnace, forming a gob and a pre-sheet, removing the gob and drawing…
The present invention relates to a process for manufacturing flat sheets of a glass-based material and to an apparatus therefor. The process comprises providing a glass preform, heating the glass preform in a furnace, forming a gob and a pre-sheet, removing the gob and drawing…
Disclosed is an optical fiber having a core with an alkali metal oxide dopant in an peak amount greater than about 0.002 wt. % and less than about 0.1 wt. %. The alkali metal oxide concentration varies with a radius of the optical fiber. By appropriately selecting the…
Microstructured optical fiber and method of making. Glass soot is deposited and then consolidated under conditions which are effective to trap a portion of the consolidation gases in the glass to thereby produce a non-periodic array of voids which may then be used to form a void…
An optical fiber is disclosed in which the core region of the optical fiber is doped with Cl and F in order to reduce the viscosity mismatch between the core region and the adjacent cladding region. In one embodiment of the invention, the optical fiber is a single-mode step…
The present invention relates to a method for producing flat sheets of glass-based material, and to an apparatus for use in the method. The method includes providing a glass preform, heating the glass preform in a furnace, forming a gob and a preform sheet, removing the gob, and…
Disclosed is an alkali-doped optical fiber perform and method for making the same. A silica glass member, such as a rod or the like is heated in a furnace chamber at a temperature of less than 75° C. below the softening point of the glass rod in an environment containing an…
A method of measuring the shape of a glass sheet is provided. The method includes positioning the glass sheet in contact with a fluid and measuring the distance between a sensor and a surface of the glass sheet at a plurality of locations on the surface thereof. The method may…
An optically active phosporus-silicate glass when pumped to directly excite Er ions, provides gain in 1565 nm to 1620 nm range and comprises in weight percent:SiO2 50 to 92%;Er2O3 0.01 to 2%;P2O5 greater than 5%; andAl2O3 0.0 to 0.3%.
A method for manufacturing an optical fiber preform and fiber. According to the method, a first glass rod is formed, preferably by an OVD method, with a refractive index delta preferably between 0.2% and 3%. A glass sleeve tube is formed, preferably by an MCVD or PVCD method.…
Microstructured optical fiber and method of making. Glass soot is deposited and then consolidated under conditions which are effective to trap a portion of the consolidation gases in the glass to thereby produce a non-periodic array of voids which may then be used to form a void…
A sacrificial structure masking method for disk drive slider assemblies. Pico size air bearing surfaces (ABS) for sliders are created by mounting parallel slider rows into a carrier. The ABS are then established by positioning a mask having a sacrificial structure within the…
A method of making a phosphosilicate fiber comprises the steps of: (i) manufacturing a preform containing phosphorus doped silica; and (ii) drawing phosphosilicate fiber from said preform at a temperature in the range of 1700° C. to 1900° C.
The present invention relates to a process for manufacturing flat sheets of a glass-based material and to an apparatus therefor. The process comprises providing a glass preform, heating the glass preform in a furnace, forming a gob and a pre-sheet, removing the gob and drawing…
The disclosed invention includes an inventive drying agent. The drying agent includes at least one halide and at least one reducing agent. Preferably, the reducing agent includes a compound that will react with an oxygen by-product of the reaction of the halide and water, or the…
A method of making an optical waveguide preform includes forming a preform including a first portion and a second radial portion, wherein the second portion includes a dopant, and wherein the first portion exhibits a density greater than the second portion. The method further…
Disclosed is an alkali-doped optical fiber preform and method for making the same. A silica glass member, such as a rod or the like is heated in a furnace chamber at a temperature of less than 75 C below the softening point of the glass rod in an environment containing an alkali…
Microstructured optical fiber and method of making. Glass soot is deposited and then consolidated under conditions which are effective to trap a portion of the consolidation gases in the glass to thereby produce a non-periodic array of voids which may then be used to form a void…
A method of manufacturing an optical waveguide preform includes providing a first process gas atmosphere to a soot preform contained in a vessel. The first atmosphere is held in the vessel for a first reacting time sufficient to at least partially dope or dry the soot preform.…