WO 2008/032503 A1#14308277 Most Cited · 7 citations0.4/yr · PR 2.76PendingWO · Application
Iron-based soft magnetic powder for dust core, method for producing the same and dust core

Disclosed is an iron powder for dust core having excellent mechanical strength, wherein effective insulation is achieved between iron powder particles even when the amount of an insulating material is reduced for realizing high-density molding. This iron powder for dust core is…

US 8,236,087 B2#27147992 Most Cited · 4 citations0.3/yr · PR 1.09ActiveUS · Utility
Powder core and iron-base powder for powder core
Inventors: Mitani Hiroyuki, Akagi Nobuaki, Houjou Hirofumi, Ishihara Chio, Iwakiri MakotoAssignee: Mitani Hiroyuki, Akagi NobuakiFiled 2007-09-11 · Granted 2012-08-07

The present invention relates to an iron-base powder for a powder core, wherein when cross-sections of at least 50 iron-base powders are observed and a crystal grain size distribution containing at least a maximum crystal grain size is determined by measuring a crystal grain…

US 8,445,105 B2#27167431 Most Cited · 4 citations0.3/yr · PR 1.09ActiveUS · Utility
Iron-based soft magnetic powder for dust core, method for production thereof, and dust core
Inventors: Mitani Hiroyuki, Akagi Nobuaki, Houjou Hirofumi, Ishihara Chio, Iwakiri MakotoAssignee: Mitani Hiroyuki, Akagi NobuakiFiled 2007-08-02 · Granted 2013-05-21

An iron-based magnetic powder for dust cores has layers of phosphoric acid-based film and silicone resin film sequentially formed on the surface thereof. The phosphoric acid-based film contains at least one element selected from the group consisting of Co, Na, S, Si, and W. The…

WO 2008/032707 A1#34902407 Most Cited · 2 citations0.1/yr · PR 1.46PendingWO · Application
Powder magnetic core and iron-base powder for powder magnetic core

This invention relates to an iron-base powder for a power magnetic core. In the iron-base powder for a powder magnetic core, when a crystal grain size distribution including at least the maximum crystal grain diameter is determined by observing at least 50 ion-base powder cross…