Aqueous dispersion obtainable by placing in water an aggregated titanium dioxide powder having a specific surface area of from 20 to 150 m2/g in such an amount that the desired dispersion comprises at least 20 wt.% titanium dioxide, and at least one amino alcohol having from 1…
Reitz Sascha
Aqueous dispersion which comprises hydrophobized silicon dioxide particles and in each case one or more dispersing additives, a basic composition, and which is free of color pigments, inactive fillers and binders, in which the hydrophobized silicon dioxide particles have a…
Stable, pourable silicon dioxide dispersion, in which the average, number-related aggregate diameter of the silicon dioxide particles in dispersion is less than 200 nm, and which comprises at least 35 wt.% of a silicon dioxide powder, 3 to 35 wt.% of at least one polyol, 20 to…
Aqueous dispersion which contains titanium dioxide, water, at least one aminoalcohol and at least one hydroxycarboxylic acid, the titanium dioxide being present in the form of aggregated primary particles having a mean, volume-related aggregate diameter of 70 to 100 nm and the…
Stable, pourable silicon dioxide dispersion, in which the average, number-related aggregate diameter of the silicon dioxide particles in dispersion is less than 200 nm, and which comprises at least 35 wt. % of a silicon dioxide powder, 3 to 35 wt. % of at least one polyol, 20 to…
Aqueous dispersion which comprises hydrophobized silicon dioxide particles and in each case one or more dispersing additives, a basic composition, and which is free of colour pigments, inactive fillers and binders, in which the hydrophobized silicon dioxide particles have a…
Provided is a process for preparing surface-modified silicon dioxide particles with a mean particle diameter of at most 100 nm, involving (A) high-pressure grinding of a predispersion having (i) surface-modified silicon dioxide particles which are at least partly aggregated, are…
Process for preparing an alkaline dispersion of aggregated silicon dioxide particles by dividing a preliminary dispersion within a pH of 3 to 5 into at least two streams, placing these streams under a pressure of at least 50 bar and depressurizing them to a collision point, each…
Process for preparing a dispersion of surface-modified silicon dioxide particles having an average particle diameter of not more than 100 nm by high-pressure milling of a preliminary dispersion comprising a) 10% to 50% by weight of surface-modified silicon dioxide particles, b)…
Aqueous dispersion obtainable by placing in water an aggregated titanium dioxide powder having a specific surface area of from 20 to 150 m2/g in such an amount that the desired dispersion comprises at least 20 wt.% titanium dioxide, and at least one amino alcohol having from 1…
Dispersion containing aluminium oxide and water, wherein the aluminium oxide is present in the form of aggregated primary particles with a BET surface area of 20 to 200 m2/g and has a mean, volume-based aggregate diameter in the dispersion of less than 100 nm, is modified with…
Process for preparing an alkaline dispersion of aggregated silicon dioxide particles by dividing a preliminary dispersion within a pH of 3 to 5 into at least two streams, placing these streams under a pressure of at least 50 bar and depressurizing them to a collision point, each…
Process for preparing surface-modified silicon dioxide particles with a mean particle diameter of at most 100 nm, comprising the steps of: a) providing a predispersion b) high-pressure grinding of the predispersion to form a dispersion c) removing the liquid phase of the…
Process for preparing surface-modified silicon dioxide particles with a mean particle diameter of at most 100 nm, comprising the steps of: a) providing a predispersion b) high-pressure grinding of the predispersion to form a dispersion c) removing the liquid phase of the…
Process for preparing a dispersion of surface-modified silicon dioxide particles having an average particle diameter of not more than 100 nm by high-pressure milling of a preliminary dispersion comprising a) 10% to 50% by weight of surface-modified silicon dioxide particles, b)…