WO 2005/018854 A1#7001756 Most Cited · 14 citations0.7/yr · PR 2.30PendingWO · Application
Method to produce an element subject to wear, and element subject to wear thus obtained

Method to produce an element (10) subject to wear, such as a mechanical member, an abrasion or crushing tool or suchlike, comprising a metal matrix (14) and at least a core (12) of ceramic material. The method comprises a preliminary step wherein the core (12) is prepared by…

US 8,505,843 B2#40407087 Most Cited · 2 citations0.1/yr · PR 1.00ActiveUS · Utility
Crushing mill
Inventors: Veneroso Enrico, Andreussi Guido, Pontelli Eddy, Andreussi OliviaAssignee: Veneroso Enrico, Andreussi GuidoFiled 2010-11-16 · Granted 2013-08-13

A crushing mill for inert material includes a distribution unit, a crushing unit disposed below the distribution unit and a containment structure to contain the distribution unit and the crushing unit. The distribution unit receives the inert material from a feed device and…

WO 2012/004654 A1#36200882 Most Cited · 2 citations0.1/yr · PR 1.19PendingWO · Application
Method for the production of an element subject to wear, element subject to wear and temporary aggregation structure to produce said element subject to wear

Method for the production of an element subject to wear (10), comprising a metal matrix (14) and at least a core (12) of hard material. The method provides a first step in which a temporary aggregation structure (17) is prepared with at least partly open pores, which volatilize…

WO 2006/061261 A1#54198332 Most Cited · 1 citations0.1/yr · PR 0.81PendingWO · Application
Method to obtain a manganese steel alloy, and manganese steel alloy thus obtained

Method to obtain a manganese steel alloy having a percentage weight of carbon varying from about 0.5% to about 2%, a percentage weight of manganese varying from about 10% to about 20%, and a percentage weight of titanium varying from about 0.01% to about 5%. The method comprises…

US 10,357,830 B2#77530495 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for the production of an element subject to wear, element subject to wear and temporary aggregation structure to produce said element subject to wear
Inventors: Andreussi Alberto, Andreussi Primo, Veneroso Enrico, Pontelli EddyAssignee: Andreussi Alberto, Andreussi PrimoFiled 2011-07-08 · Granted 2019-07-23

The method for the production of an element subject to wear, comprising a metal matrix and at least a core of hard material. The method provides a first step in which a temporary aggregation structure is prepared with at least partly open pores, which volatilize or in any case…

US 2007292299 A1#114092454 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method to Obtain a Manganese Steel Alloy, and Manganese Steel Alloy Thus Obtained

A method to obtain a manganese steel alloy having a percentage weight of carbon varying from about 0.5% to about 2%, a percentage weight of manganese varying from about 10% to about 20%, and a percentage weight of titanium varying from about 0.01% to about 5%. The method…

US 2013115475 A1#137344989 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method for the Production of an Element Subject to Wear, Element Subject to Wear and Temporary Aggregation Structure to Produce Said Element Subject to Wear

The method for the production of an element subject to wear, comprising a metal matrix and at least a core of hard material. The method provides a first step in which a temporary aggregation structure is prepared with at least partly open pores, which volatilize or in any case…

US 8,636,857 B2#93687222 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredUS · Utility
Method to obtain a manganese steel alloy
Inventors: Andreussi Alberto, Andreussi Primo, Veneroso Enrico, Pontelli EddyAssignee: Andreussi Alberto, Andreussi PrimoFiled 2005-05-12 · Granted 2014-01-28

A method to obtain a manganese steel alloy having a percentage weight of carbon varying from about 0.5% to about 2%, a percentage weight of manganese varying from about 10% to about 20%, and a percentage weight of titanium varying from about 0.01% to about 5%. The method…

WO 2012/004654 A8#121582560 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Method for the production of an element subject to wear, element subject to wear and temporary aggregation structure to produce said element subject to wear

Method for the production of an element subject to wear (10), comprising a metal matrix (14) and at least a core (12) of hard material. The method provides a first step in which a temporary aggregation structure (17) is prepared with at least partly open pores, which volatilize…

WO 2012/004655 A1#128669249 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for the production of an element subject to wear, element subject to wear and temporary aggregation structure to produce said element subject to wear

Method for the production of an element subject to wear (10), comprising a metal matrix (14) and at least a core (12) of hard material. The method provides a first step in which a temporary aggregation structure (17) is prepared with at least partly open pores, which volatilizes…