The method is used for processing uranic and polymetallic ores. Iron(II) sulphate is added to the pulp of the uranic ore in batches of 2 to 350 kg/t of the ore. The ore is leached under conditions of the increased temperatures of 110 to 200 degrees C and pressures of 0.3 to 2.5…
Assignee / Organization
Malis Ales
0Total Forward Citations
2Indexed Patents
0Avg Citations / Patent
0Portfolio H-Index