When building-up additional material by welding the surface of the base is covered by a 0.05 to 0.8 mm layer of powdered material consisting of 0.02 to 0.2 mm sized particles with the same or lower melting point than the melting point of the additional material and then this…
Assignee / Organization
Halfar Jan
0Total Forward Citations
2Indexed Patents
0Avg Citations / Patent
0Portfolio H-Index
When building-up additional material by welding the surface of the base is covered by a 0.05 to 0.8 mm layer of powdered material consisting of 0.02 to 0.2 mm sized particles with the same or lower melting point than the melting point of the additional material and then this…