The present invention relates to a new polymer composition suitable for a semiconductive devices. Moreover, the present invention is related to a process for producing said composition as well as to a use of said composition. Further, the invention is also related to an article,…
Friel David
The present invention relates to a new polymer composition suitable for a semiconductive devices. Moreover, the present invention is related to a process for producing said composition as well as to a use of said composition. Further, the invention is also related to an article,…
Cable layer comprising a propylene polymer composition comprising (a) a polypropylene (A) (b) an elastomeric copolymer (E) comprising units derived from propylene and ethylene and/or C4 to C20 α-olefin and (c) a polar ethylene polymer (C) wherein the cable layer and/or the…
The present invention relates to a polypropylene composition showing a high melt flow rate and high melt strength while maintaining high impact strength. The composition of the present invention is obtainable by using a low molecular weight linear isotactic polypropylene as melt…
The present invention relates to a polypropylene composition showing a high melt flow rate and high melt strength while maintaining high impact strength. The composition of the present invention is obtainable by using a low molecular weight linear isotactic polypropylene as melt…
Described herein are polymer compositions useful as a semiconductive layer suitable for cables. The polymer compositions include (a) a heterophasic copolymer of propylene, (b) a polar copolymer having a polar comonomer having polar groups, (c) a solid conductive filler, and…
Cable layer comprising a propylene polymer composition comprising (a) a polypropylene (A) (b) an elastomeric copolymer (E) comprising units derived from propylene and ethylene and/or C4 to C20 α-olefin and (c) a polar ethylene polymer (C) wherein the cable layer and/or the…
The present invention relates to a polypropylene composition showing a high melt flow rate and high melt strength while maintaining high impact strength. The composition of the present invention is obtainable by using a low molecular weight linear isotactic polypropylene as melt…
The present invention relates to a polypropylene which has - a melt flow rate MFR(230°C, 2.16 kg) of at least 13 g/10 min, - an amount of xylene solubles XS of 6.0 wt% or less, and - a crystalline fraction, wherein at least 10 % of the crystalline fraction melts the temperature…
The present invention relates to a polypropylene which has—a melt flow rate MFR(230° C., 2.16 kg) of at least 13 g/10 min,—an amount of xylene solubles XS of 6.0 wt % or less, and—a crystalline fraction, wherein at least 10% of the crystalline fraction melts the temperature…
The present invention relates to a polypropylene which has—a melt flow rate MFR(230° C., 2.16 kg) of at least 13 g/10 min,—an amount of xylene solubles XS of 6.0 wt % or less, and—a crystalline fraction, wherein at least 10% of the crystalline fraction melts the temperature…