In a method for producing a lead-free sliding bearing, a copper-based material comprising a total of 0.1% to 3% of the elements aluminum, magnesium, silicon, titanium, zircon, and chromium is sintered. Additionally, up to 15% tin can be included in order to ensure optimal…
Assignee / Organization
Broniszewski Andrzej
8Total Forward Citations
3Indexed Patents
3Avg Citations / Patent
2Portfolio H-Index
In a method for producing a lead-free sliding bearing, a copper-based material comprising a total of 0.1% to 3% of the elements aluminum, magnesium, silicon, titanium, zircon, and chromium is sintered. Additionally, up to 15% tin can be included in order to ensure optimal…