{"pub_number":"US4502209A","doc_number":"4502209","country":"US","kind_code":"A","patent_type":"utility","status":"expired","title":"Forming low-resistance contact to silicon","abstract_text":"Annealing a titanium-rich carbide film deposited on silicon produces, in a single processing step, both a stable titanium silicide contact and a titanium carbide diffusion barrier between the silicide and a subsequently formed overlying layer of aluminum. Reliable low-resistance contacts to VLSI devices are thereby provided in a cost-effective fabrication sequence. Other metallization systems, comprising a silicide and a diffusion barrier to aluminum formed in a single processing step, are also described.","claims":[{"number":1,"text":"A method of making a semiconductor device, comprising the steps of depositing a film of A x  B on a surface of a device structure that includes silicon surface regions, where A is selected from the group consisting of titanium, hafnium, zirconium, tantalum and niobium, and B is selected from the group consisting of carbon, nitrogen and boron,   and heating said structure to convert those portions of the film that overlie silicon surface regions into a two-layer metallization comprising a layer of ASi 2  and an overlying layer of A y  B, where x is both greater than one and greater than y.","independent":true},{"number":2,"text":"A method as in claim 1 wherein 1&lt;x&lt;5, and further comprising depositing a layer of aluminum on said film,   and correspondingly patterning said layer and unconverted portions of said underlying film to form composite-metallization elect","independent":false,"depends_on":[1]}],"description":"","inventors":[{"name":"Eizenberg Moshe","slug":"eizenberg-moshe","country":"IL"},{"name":"Murarka Shyam P","slug":"murarka-shyam-p","country":"US"}],"assignees":[{"name":"At & T Bell Lab","slug":"at-t-bell-lab","country":"US"}],"examiners":["Hearn Brian E.","Hey David A."],"cpc_codes":["H01L 21/28518","H01L 21/76843","H01L 23/53223","H01L 2924/0002","H10D 62/83","H10D 64/62"],"ipc_codes":["H01L 21/28","H01L 21/285","H01L 21/768","H01L 23/532","H01L 29/45","H01L 29/78"],"filing_date":"1983-08-31","pub_date":"1985-03-05","grant_date":"1985-03-05","priority_date":"1983-08-31","expiration_date":"2003-08-31","application_number":"US-52807483-A","family_id":"FAM-24104162","family_members":[],"citations_made":[{"pub_number":"US3714520A","category":"SEA"},{"pub_number":"US3794516A","category":"SEA"},{"pub_number":"US3879746A","category":"SEA"}],"non_patent_literature":["\"Interaction of Reactively Sputtered Titanium Carbide Thin Films with Si, SiO2 Ti, TiSi2, and Al\", J. Appl. Phys., 54(6), Jun. 1983, M. Eizenberg et al, pp. 3195-3199.","Interaction of Reactively Sputtered Titanium Carbide Thin Films with Si, SiO 2 Ti, TiSi 2 , and Al , J. Appl. Phys., 54(6), Jun. 1983, M. Eizenberg et al, pp. 3195 3199."],"drawings_count":0,"source_id":"google_patents_public","upstream_forward_citations":0,"metrics":{"forward_citations":75,"indexed_forward_citations":75,"backward_citations":3,"npl_citations":2,"citations_per_year":1.83,"pagerank":41.84695053100586,"citation_rank":422833,"pagerank_rank":96550,"velocity_rank":2425766,"family_citations":75}}