{"pub_number":"US12349377B2","doc_number":"12349377","country":"US","kind_code":"B2","patent_type":"utility","status":"active","title":"Preparation method for semiconductor structure involving the replacement of dielectric layer with gate","abstract_text":"According to the preparation method for a semiconductor structure provided in the present application, a selective epitaxial growth method is used, without etching the n-type semiconductor layer and the p-type semiconductor layer, thus avoiding problems such as uncontrollable etching depth and damaged etched surface, which effectively reduces gate leakage, maintains low resistance in a channel region, suppresses current collapse, and improves reliability and stability of a device.","claims":[{"number":1,"text":"A preparation method for a semiconductor structure, comprising: sequentially preparing a channel layer, a barrier layer, and a p-type semiconductor layer on a substrate; preparing a dielectric layer in a gate region of a first layer above the p-type semiconductor layer, a material of the dielectric layer comprising at least one of SiO 2 and Al 2 O 3, a lower surface of the dielectric layer being in contact with an upper surface of the p-type semiconductor layer; preparing an n-type semiconductor layer in a region other than the gate region of the first layer above the p-type semiconductor layer by a selective epitaxial growth method, a lower surface of the n-type semiconductor layer being in contact with the upper surface of the p-type semiconductor layer, and the lower surface of the n-type semiconductor layer being in a same plane as the lower surface of the dielectric layer; and activating a p-type impurity in the p-type semiconductor layer covered by the dielectric layer, to form an active region, wherein when forming the active region, hydrogen component in the p-type semiconductor layer overflows through the dielectric layer to activate the p-type impurity in the p-type semiconductor layer, and for the p-type semiconductor layer covered by the n-type semiconductor layer, due to blocking of the n-type semiconductor layer, hydrogen component cannot overflow but bond with the p-type impurity in the p-type semiconductor layer, and the p-type impurity in the p-type semiconductor layer cannot be activated, forming an inactive region, wherein the preparing a dielectric layer in a gate region of a first layer above the p-type semiconductor layer comprises: forming a dielectric layer in the first layer above the p-type semiconductor layer; and etching the dielectric layer in a region other than the gate region of the first layer above the p-type semiconductor layer.","independent":true},{"number":2,"text":"The preparation method for a semiconductor structure according to claim 1, further comprising: removing the dielectric layer, and preparing a gate above the active region of the p-type semiconductor layer.","independent":false,"depends_on":[1]},{"number":3,"text":"The preparation method for a semiconductor structure according to claim 2, wherein the dielectric layer is removed by a wet etching method.","independent":false,"depends_on":[2]},{"number":4,"text":"The preparation method for a semiconductor structure according to claim 1, further comprising: preparing a source and a drain respectively in a source region and a drain region, wherein the source and the drain penetrate the n-type semiconductor layer and the p-type semiconductor layer.","independent":false,"depends_on":[1]},{"number":5,"text":"The preparation method for a semiconductor structure according to claim 1, wherein the preparing a source and a drain respectively in a source region and a drain region comprises: forming a groove by etching on two sides of a gate, wherein the groove penetrates through the n-type semiconductor layer and the p-type semiconductor layer, and stops at the barrier layer; and depositing metal in the groove to prepare the source and the drain.","independent":false,"depends_on":[1]},{"number":6,"text":"The preparation method for a semiconductor structure according to claim 5, wherein an etching method of the groove is a dry etching method.","independent":false,"depends_on":[5]},{"number":7,"text":"The preparation method for a semiconductor structure according to claim 1, wherein a method of forming the active region comprises annealing a semiconductor structure.","independent":false,"depends_on":[1]},{"number":8,"text":"The preparation method for a semiconductor structure according to claim 7, wherein the annealing comprises performing annealing in a hydrogen-free environment.","independent":false,"depends_on":[7]},{"number":9,"text":"The preparation method for a semiconductor structure according to claim 1, wherein the p-type semiconductor layer and the n-type semiconductor layer comprise a GaN-based semiconductor.","independent":false,"depends_on":[1]},{"number":10,"text":"The preparation method for a semiconductor structure according to claim 1, wherein before preparing the channel layer, the preparation method further comprises: sequentially forming a nucleation layer and a buffer layer on the substrate.","independent":false,"depends_on":[1]},{"number":11,"text":"The preparation method for a semiconductor structure according to claim 10, wherein the nucleation layer comprises one or more of AlN, AlGaN, and GaN.","independent":false,"depends_on":[10]},{"number":12,"text":"The preparation method for a semiconductor structure according to claim 10, wherein the buffer layer comprises one or more of GaN, AlGaN, and AlInGaN.","independent":false,"depends_on":[10]},{"number":13,"text":"The preparation method for a semiconductor structure according to claim 1, wherein the channel layer, the barrier layer and the p-type semiconductor layer are grown in situ, or be grown by Atomic Layer Deposition (ALD), Chemical Vapor Deposition (CVD), Molecular Beam Epitaxy (MBE), Plasma Enhanced Chemical Vapor Deposition (PECVD), Low Pressure Chemical Vapor Deposition (LPCVD), Metal-Organic Chemical Vapor Deposition (MOCVD), or a combination thereof.","independent":false,"depends_on":[1]}],"claim_stats":{"total":13,"independent":1,"dependent":12},"description":"CROSS-REFERENCE TO RELATED APPLICATIONS\nThis application is a continuation of International Application No. PCT/CN2019/087262 filed on May 16, 2019, the disclosure of which is hereby incorporated by reference in its entirety.\nTECHNICAL FIELD\nThis application relates to the field of microelectronics technologies, and in particular, to a preparation method for a semiconductor structure.\nBACKGROUND\nHigh Electron Mobility Transistor (HEMT) is a heterojunction field-effect transistor. Taking an AlGaN/GaN heterostructure as an example, since there is a strong two-dimensional electron gas in the AlGaN/GaN heterostructure, and an AlGaN/GaN HEMT is generally a depletion device, it is difficult to implement an enhancement-mode device. In addition, an application of a depletion device has certain limitations in many cases. For example, in an application of a power switching device, an enhancement-mode (normally-off mode) switching device is required. An enhancement-mode gallium nitride switching device is mainly used in a high-frequency device, a power switching device, a digital circuit or the like, and research into the enhancement-mode gallium nitride switching device is of great importance.\nTo implement the enhancement-mode gallium nitride switching device, it is necessary to find a suitable method to reduce concentration of a channel carrier under a gate when a gate voltage is zero, for example, by disposing a p-type semiconductor material in a gate region. However, the inventor found that this method has at least the following defects:\nTo dispose a p-type semiconductor material in a gate region, it is necessary to selectively etch the p-type semiconductor in other regions other than the gate, while it is difficult to control an etching process for precise thickness in an epitaxial direction, and it is easy to overetch the p-type semiconductor, and thus a semiconductor material below the p-type semiconductor is etched. In addition, the defects caused by etching will cause","inventors":[{"name":"Kai Cheng","slug":"kai-cheng","city":"Suzhou","country":"CN"}],"assignees":[{"name":"ENKRIS SEMICONDUCTOR, INC.","slug":"enkris-semiconductor-inc","country":"CN"}],"examiners":[],"cpc_codes":["H01L 21/2258","H01L 21/3245","H10D 30/015","H10D 30/475","H10D 62/60"],"ipc_codes":["H01L 21/225","H01L 21/324","H10D 30/01","H10D 30/47","H10D 62/60"],"filing_date":"2021-11-15","pub_date":"2025-07-01","grant_date":"2025-07-01","expiration_date":"2041-11-15","family_members":[],"citations_made":[{"pub_number":"US5701019A","category":"applicant"},{"pub_number":"US20090162999A1","category":"examiner"},{"pub_number":"US20090212325A1","category":"applicant"},{"pub_number":"US20120211760A1","category":"examiner"},{"pub_number":"US20140264379A1","category":"examiner"},{"pub_number":"US20150021662A1","category":"examiner"},{"pub_number":"US20160211357A1","category":"applicant"},{"pub_number":"US20170278961A1","category":"examiner"},{"pub_number":"US20170309712A1","category":"examiner"},{"pub_number":"US20180090911A1","category":"examiner"},{"pub_number":"US20190097034A1","category":"examiner"},{"pub_number":"US20190311914A1","category":"examiner"},{"pub_number":"US20220140126A1","category":"examiner"},{"pub_number":"CN103337516A","category":"applicant"},{"pub_number":"CN108346695A","category":"applicant"},{"pub_number":"CN108565283A","category":"applicant"},{"pub_number":"CN108962752A","category":"applicant"},{"pub_number":"JP2011146613A","category":"applicant"}],"non_patent_literature":["First Office Action issued in counterpart Chinese Patent Application No. 201980096456.3, dated Apr. 27, 2022.","International Search Report issued in corresponding PCT Application No. PCT/CN2019/087262, dated Jan. 19, 2020.","Written Opinion issued in corresponding PCT Application No. PCT/CN2019/087262, dated Jan. 19, 2020."],"drawings_count":3,"source_id":"uspto_patent_grants","upstream_forward_citations":0,"metrics":{"forward_citations":0,"indexed_forward_citations":0,"backward_citations":18,"npl_citations":3,"citations_per_year":0.0,"pagerank":0.0,"citation_rank":3505210,"pagerank_rank":3505210,"velocity_rank":3505210,"family_citations":0}}